Polymer Property : Thermal Conductivity = 0.490 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.390 - 0.490 W/m-K

@Temperature 600 °C
2.71 - 3.40 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Gouda Vuurvast FI 35-12 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.