Polymer Property : Thermal Conductivity = 0.3024 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.3024 W/m-K

@Temperature 540 °C
2.095 BTU-in/hr-ft²-°F

@Temperature 1000 °F
Chosun Refractories GUN-110L Light-Weight Gunning Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 0.3024 W/m-K

@Temperature 260 °C
2.095 BTU-in/hr-ft²-°F

@Temperature 500 °F
Chosun Refractories INCT-110N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).
Thermal Conductivity 0.3024 W/m-K

@Temperature 260 °C
2.095 BTU-in/hr-ft²-°F

@Temperature 500 °F
Chosun Refractories INCT-120N Light-Weight Castable
Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET).