Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.174 W/m-K @Temperature 540 °C |
1.21 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Chosun Refractories INCT-100S Light-Weight Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |
|||
Thermal Conductivity | 0.174 - 0.233 W/m-K @Temperature 540 °C |
1.21 - 1.61 BTU-in/hr-ft²-°F @Temperature 1000 °F |
|
Chosun Refractories MIX-2 Light-Weight Gunning Castable Information provided by Chosun Refractories via Korea Institute of Ceramic Engineering and Technology (KICET). |