Polymer Property : Thermal Conductivity = 0.154 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.154 W/m-K

@Temperature 35.0 °C
1.07 BTU-in/hr-ft²-°F

@Temperature 95.0 °F
Dow VORANOL™ 4703 Polyether Polyol
VORANOL™ 4703 polyether polyol is a nominal 5000 molecular weight, high reactivity capped triol. It has a high primary hydroxyl content making it suitable for use in making all types of high resil..