Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.1504 W/m-K @Temperature 23.9 °C |
1.044 BTU-in/hr-ft²-°F @Temperature 75.0 °F |
|
Paratherm Corporation Paratherm™ LR Heat Transfer Fluid Paratherm LR™ heat transfer fluid is an aliphatic-hydrocarbon based heat transfer fluid designed for use in closed-loop, liquid phase heating and cooling systems up to 450°F in electric and steam .. |