Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.1453 W/m-K @Temperature -45.6 °C |
1.008 BTU-in/hr-ft²-°F @Temperature -50.0 °F |
|
Paratherm Corporation Paratherm™ CR Heat Transfer Fluid Paratherm CR® heat transfer fluid is a blend of synthetic components formulated to provide superior cooling performance in closed-loop heat-transfer systems operating down to -88°C (-127°F) yet i.. |
|||
Thermal Conductivity | 0.1453 W/m-K @Temperature 37.8 °C |
1.008 BTU-in/hr-ft²-°F @Temperature 100 °F |
|
Duratherm 630 Paraffinic Heat Transfer Fluid Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F.. |
|||
Thermal Conductivity | 0.1453 W/m-K @Temperature 37.8 °C |
1.008 BTU-in/hr-ft²-°F @Temperature 100 °F |
|
Duratherm FG Paraffinic Heat Transfer Fluid Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac.. |