Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.135 W/m-K @Temperature -17.8 °C |
0.936 BTU-in/hr-ft²-°F @Temperature 0.000 °F |
|
Paratherm Corporation Paratherm™ GLT™ Heat Transfer Fluid Paratherm GLT™ Heat Transfer Fluid is an alkylated aromatic based heat transfer fluid formulated for closed loop liquid phase heating systems to 550°F using fired heaters and to 575°F in waste-he.. |
|||
Thermal Conductivity | 0.135 W/m-K @Temperature 0.000 °C |
0.938 BTU-in/hr-ft²-°F @Temperature 32.0 °F |
|
ChevronTexaco Texatherm® Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging .. |
|||
Thermal Conductivity | 0.135 W/m-K @Temperature 260 °C |
0.936 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Duratherm 630 Paraffinic Heat Transfer Fluid Duratherm 630 - rated to 630°F it has the highest rated bulk temperature of petroleum based thermal fluids. Duratherm 630 is engineered for applications requiring high temperature stability (630°F.. |
|||
Thermal Conductivity | 0.135 W/m-K @Temperature 260 °C |
0.936 BTU-in/hr-ft²-°F @Temperature 500 °F |
|
Duratherm FG Paraffinic Heat Transfer Fluid Duratherm FG - thermal oil rated to 620°F it is engineered and manufactured to comply with the demands of food grade applications. NSF registered, meets USDA requirements for incidental food contac.. |