Thermal Properties Metric English Comments
Thermal Conductivity 0.132 W/m-K

@Temperature 200 °C
0.916 BTU-in/hr-ft²-°F

@Temperature 392 °F
Mean temp.; ASTM C-182
Skamol Group Moler POROS Insulating Block
SKAMOL Moler insulating bricks & blocks have the following characteristics: Max. service temperature: Up to 1000°C (1832°F)Back-up insulation Excellent insulating propertiesHigh mechanical str..
Thermal Conductivity 0.132 W/m-K

@Temperature 50.0 °C
0.913 BTU-in/hr-ft²-°F

@Temperature 122 °F
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..
Thermal Conductivity 0.132 W/m-K

@Temperature 40.0 °C
0.918 BTU-in/hr-ft²-°F

@Temperature 104 °F
ChevronTexaco Texatherm®
Texaco Texatherm and Texatherm 22 deliver value through:Excellent thermal efficiency and stability — Long oil life is assured by outstanding thermal and oxidation stability which prevents sludging ..