Polymer Property : Thermal Conductivity = 0.103 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.103 W/m-K

@Temperature 100 °C
0.715 BTU-in/hr-ft²-°F

@Temperature 212 °F
Pyrotek Pyrite N-17 Refractory Board
Pyrotek N-17 is a graphite fiber reinforced, high purity, calcium silicate board developed exclusively for the non-ferrous casting industry. The patented formulation of Pyrotek N-17 makes it good i..