Polymer Property : Thermal Conductivity = 0.1025 W/m-K Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.1025 W/m-K

@Temperature 220 °C
0.7114 BTU-in/hr-ft²-°F

@Temperature 428 °F
ASTM D1674
DuPont™ Nomex® Type 993, 160 mil Nominal Thickness Medium-Density Aromatic Nylon Pressboard
Type 993 is a medium-density pressboard which offers a balance of rigidity and conformability along with outstanding saturability and excellent properties in air and oil. Typical applications includ..