Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0880 W/m-K @Temperature 93.0 °C |
0.611 BTU-in/hr-ft²-°F @Temperature 199 °F |
|
Pyrotek I-28 Insulating Board Pyrotek's I-28 is a low density hydrous calcium silicate board which features exceptional strength and low thermal conductivity. Inorganic and incombustible, I-28 also contains no RCF's.A.. |