Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Thermal Conductivity 0.0450 W/m-K

@Temperature 600 °C
0.312 BTU-in/hr-ft²-°F

@Temperature 1110 °F
Unifrax Excelfrax® 1900 Panel Microporous Insulation
Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo..
Thermal Conductivity 0.0450 W/m-K

@Temperature 92.0 °C
0.312 BTU-in/hr-ft²-°F

@Temperature 198 °F
1 in. blanket, 9.98 pcf; ASTM C177
Zircar Refractory Composites SB-2000 SILICA BLANKET
ZIRCAR Silica Blanket Type SB-2000 is a high temperature insulation blanket made of mechanically interlocked continuous filament amorphous silica fibers with useful properties to temperatures of 110..