Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0420 W/m-K @Temperature 537 °C |
0.291 BTU-in/hr-ft²-°F @Temperature 999 °F |
Standard |
Pyrotek MT-29P Microporous Panel Insulation MT-29P is a unique panel insulation which offers exceptionally low thermal conductivity. The exterior of the panel is a glass fabric which maximizes the strength of the rigid interior panel.Applica.. |
|||
Thermal Conductivity | 0.0420 W/m-K @Temperature 537 °C |
0.291 BTU-in/hr-ft²-°F @Temperature 999 °F |
Standard |
Pyrotek MT-29Q Quilted Microporous Insulation MT-29Q is quilted to encapsulate its microporous core between glass cloth. The result is a flexible insulating material which offers exceptionally low thermal conductivity. The quilting maintains .. |
|||
Thermal Conductivity | 0.0420 W/m-K @Temperature 537 °C |
0.291 BTU-in/hr-ft²-°F @Temperature 999 °F |
Standard |
Pyrotek MT-29L Microporous Ladle Lining Insulation MT-29L is a microporous insulation material covered with a flexible glass fabric. Parallel-stitched for ease of handling during installation, it is designed for use between ladle shells and the bac.. |
|||
Thermal Conductivity | 0.0420 W/m-K @Temperature 50.0 °C |
0.291 BTU-in/hr-ft²-°F @Temperature 122 °F |
@ 110 kg/m³; ASTM C177, ISO 8302, DIN EN-12667:2001-05 |
Microtherm Group MT Thermosphere® Moldable Insulation Paste MT Thermosphere® is a low density temperature resistant paste with excellent thermal insulation properties from cryogenic to high temperature exposure. It is a perfectly seamless insulation syste.. |
|||
Thermal Conductivity | 0.0420 W/m-K @Temperature 800 °C |
0.291 BTU-in/hr-ft²-°F @Temperature 1470 °F |
DIN 51046 |
Unifrax Excelfrax® 1800 Flexliner Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Thermal Conductivity | 0.0420 W/m-K @Temperature 537 °C |
0.291 BTU-in/hr-ft²-°F @Temperature 999 °F |
Standard |
Pyrotek MT-29B Microporous Insulating Board MT-29B has the low thermal conductivity. Its cellular structure contributes to its low-weight, good compressive strength, and low shrinkage at high temperatures.ApplicationsBackup insulation for: T.. |