Thermal Properties | Metric | English | Comments |
---|---|---|---|
Thermal Conductivity | 0.0210 W/m-K @Temperature 200 °C |
0.146 BTU-in/hr-ft²-°F @Temperature 392 °F |
DIN 51046 |
Unifrax Excelfrax® 1800 Board Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |
|||
Thermal Conductivity | 0.0210 W/m-K @Temperature 20.0 °C |
0.146 BTU-in/hr-ft²-°F @Temperature 68.0 °F |
DIN 51046 |
Unifrax Excelfrax® 1800 Flexliner Microporous Insulation Unifrax Corporation's Excelfrax® product line, based on advanced microporous insulation technology, is a family of products which all exhibit superior insulating characteristics. Excelfrax micropo.. |