Thermal Properties Metric English Comments
Vicat Softening Point 53.0 °C

@Load 5.001 kg
127 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYelast TPE HJ752 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 53.0 °C

@Load 5.001 kg
127 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYelast TPE HJ753 Thermoplastic Elastomer, PP/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 53.0 °C

@Load 5.001 kg
127 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP HJ752 Polypropylene/Elastomer, Mineral Reinforced
Information provided by Polykemi AB
Vicat Softening Point 53.0 °C

@Load 5.001 kg
127 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PP HJ752 UV Polypropylene/Elastomer, Mineral Reinforced
Information provided by Polykemi AB