Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 47.0 °C @Load 5.10 kg |
117 °F @Load 11.2 lb |
ISO 306 |
Borealis Borcom™ WE007AE Polypropylene Borcom™ WE007AE is a polypropylene microcomposite intended for injection molding. The product is available in natural color. This material has an excellent balance between impact strength and stif.. |