Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 189 °C @Load 5.001 kg |
372 °F @Load 11.03 lb |
50°C/h; ISO 306 |
Polykemi AB POLYshine PBT C213 GF15 FR PBT, Glass Fiber-Reinforced, Flame Retardant Information provided by Polykemi AB |
|||
Vicat Softening Point | 189 °C @Load 0.999 kg |
372 °F @Load 2.20 lb |
50°C/hr; ISO 306 |
Cossa Polimeri ESTABLEND PA 1040 GF HI ABS / Nylon 6 Blend, 20% Glass Filled ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.20% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi.. |