Polymer Property : Vicat Softening Point = 307 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 153 °C

@Load 1.00 kg
307 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH GK8020D Polypropylene Homopolymer, Glass Reinforced, Detergent Resistant
Information provided by Polykemi AB
Vicat Softening Point 153 °C

@Load 1.00 kg
307 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPHC GF3020 PB7 Polypropylene, Glass Fibre-Reinforced, Chemically Coupled
Information provided by Polykemi AB
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
ISO 306
Borealis HF700SA Polypropylene
HF700SA is a polypropylene homopolymer intended for injection molding. This material has excellent balanced mechanical properties and is easy to process. Applications: household applications.Infor..
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
ISO 306
Borealis HK060AE Polypropylene Homopolymer
HK060AE is a special low viscosity polypropylene homopolymer compound developed to fit the production of glass matt reinforced thermoplastics. This material is also suitable as base resin for the pr..
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
50°C per hour; ISO 306
Total PPH 12020 Polypropylene Homopolymer, Injection Molding
Polypropylene PPH 12020 is a clarified high fluidity homopolymer with a melt flow index of 60 g/10 min.Polypropylene PPH 12020 has been designed with a very high stiffness and an outstanding transpa..
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
50°C per hour; ISO 306
Total PPH 4026 Polypropylene Homopolymer, Film
Polypropylene PPH 4026 is a homopolymer polypropylene with a Melt Flow index of 3 g/10 min for the cast extrusion of films with outstanding stiffness and heat resistance.Polypropylene PPH 4026 is in..
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
50°C per hour; ISO 306
Total PPH 4026 Polypropylene Homopolymer, Sheet Extrusion and Thermoforming
This grade belongs to the Total Ecosolution line.Polypropylene PPH 4026 is a polypropylene homopolymer specifically developed to offer outstanding processability for sheet extrusion and thermoformin..
Vicat Softening Point 153 °C

@Load 1.02 kg
307 °F

@Load 2.25 lb
50°C per hour; ISO 306
Total PPM H350 Polypropylene, Homopolymer Medical Grade
Polypropylene PPM H350 is a homopolymer with a Melt Flow Index of 35 g/10 min recommended for the manufacture of medical packaging and medical devices, to the exclusion of implants.Polypropylene PPM..