Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 149 °C @Load 1.00 kg |
300 °F @Load 2.21 lb |
50°C/h; ISO 306 |
Polykemi AB POLYfill PP EIP5025 F VT2 Polypropylene, Mineral Reinforced, Extrusion grade, Low CLTE Information provided by Polykemi AB |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
50°C/h; ISO 306 |
Covestro Makrolon® 3100 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• General purpose• Hig.. |
|||
Vicat Softening Point | 149 °C @Load 5.10 kg |
300 °F @Load 11.2 lb |
120°C/h; ISO 306 |
Covestro Makrolon® 3258 Polycarbonate Main characteristics:• High toughness• Good heat resistance• Glass-like transparency, optical quality• High dimensional accuracy and stabilityGrade characteristics:• Medical devices - bioc.. |