Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Vicat Softening Point = 235 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 113 °C

@Load 5.00 kg
235 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND 4500 Polycarbonate ABS Blend
Polycarbonate and Acrylonitrile Butadiene Styrene blendGood impact resistance at low temperature, high glossInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 113 °C

@Load 0.999 kg
235 °F

@Load 2.20 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTADIENE 0417 GIF Acrylonitrile Butadiene Styrene, 17% Glass Filled
ABS with 17% glass fiber reinforcementGood thermal resistance, good processabilityInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 113 °C

@Load 5.10 kg
235 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® T50 BBS083 PC/ABS Blend
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Injection molding• Goo..
Vicat Softening Point 113 °C

@Load 1.00 kg
235 °F

@Load 2.20 lb
120°C/hr; ASTM D1525
Diamond Polymers Centrex® 925 Injection Molding Grade
Centrex 925 resin is a soft-flow, high-gloss, molding grade of Polycarbonate / ASA (acrylonitrile-styrene-acrylate) blend. It is an injection molding grade with a good balance of physical properties..
Vicat Softening Point 113 °C

@Load 1.00 kg
235 °F

@Load 2.20 lb
50°C/hr; ISO 306
Chi Mei Polylac® PA-777B ABS - High Heat
High Heat Impact