Polymer Property : Vicat Softening Point = 228 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 109 °C

@Load 1.00 kg
228 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYabs SN0 ABS
Information provided by Polykemi AB
Vicat Softening Point 109 °C

@Load 1.00 kg
228 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-117 SAN
Injection Molding
Vicat Softening Point 109 °C

@Load 1.00 kg
228 °F

@Load 2.20 lb
120°C/hr; ISO 306
Chi Mei Kibisan® PN-117C SAN
High Clarity
Vicat Softening Point 109 °C

@Load 5.00 kg
228 °F

@Load 11.0 lb
50°C/hr; ISO 306
Cossa Polimeri ESTABLEND PA 1424 GF HI ABS / Nylon 6 Blend, 12% Glass Filled
ESTABLEND PA is a blend of acrylonitrile butadiene styrene and polyamide 6.12% glass fiber reinforcedHigh impact strength, high chemical resistance, excellent heat resistance, high dimensional stabi..