Vicat Softening Point 205 °C

@Load 1.02 kg
401 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Terblend® S NM-31 ASA / PA
Terblend® S is a UV-stabilized ASA/PA blend with high impact strength, easy flow and pronounced color fastness. It is especially suitable for unpainted highly UV-exposed automotive interior parts..
Vicat Softening Point 205 °C

@Load 5.00 kg
401 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM Epinyl PA 6 GF 30 ATP Polyamide 6, 30% Glass
Characteristics: medium viscosity, 30% glass fibre, good toughness
Vicat Softening Point 205 °C

@Load 5.00 kg
401 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM Epinyl PA 6 GF 30 H Polyamide 6, 30% Glass, Heat Stabilized
Characteristics: medium viscosity, 30% glass fibre, heat stabilized
Vicat Softening Point 205 °C

@Load 5.00 kg
401 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM Epinyl PA 6 GF 30 Polyamide 6, 30% Glass
Characteristics: medium viscosity, 30% glass fibre, excellent mechanical properties
Vicat Softening Point 205 °C

@Load 0.999 kg
401 °F

@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
EPICHEM Epinyl PA 6 Polyamide 6
Characteristics: medium viscosity, good mechanical properties
Vicat Softening Point 205 °C

@Load 5.00 kg
401 °F

@Load 11.0 lb
120°C/min; ASTM D1525/B, ISO 306/B
EPICHEM PA 6 GF 30 Polyamide 6, 30% Glass
Characteristics: medium viscosity, 30% glass fibre filled
Vicat Softening Point 205 °C

@Load 0.999 kg
401 °F

@Load 2.20 lb
120°C/min; ASTM D1525/A, ISO 306/A
EPICHEM PA 6 Polyamide 6
Characteristics: medium viscosity, general purpose
Vicat Softening Point 205 °C

@Load 5.10 kg
401 °F

@Load 11.2 lb
dry; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF20 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 20% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Vicat Softening Point 205 °C

@Load 5.10 kg
401 °F

@Load 11.2 lb
dry; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF30 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 30% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..
Vicat Softening Point 205 °C

@Load 5.10 kg
401 °F

@Load 11.2 lb
cond.; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF30 TF15 Polyamide 6 - Improved Slip Properties
Medium viscosity injection molding grade, also used for compounding, for production of monofilament, bristles and fibers.Low wear and low friction grade, contains molybdenum disulfide, PTFE.Tarnamid..
Vicat Softening Point 205 °C

@Load 5.10 kg
401 °F

@Load 11.2 lb
dry; ISO 306
Azoty Tarnow™ Tarnamid® T-27 GF40 FRV0 Polyamide 6 - Flame Retarded, Reinforced
Flame retarded grades, flammability class V0, reinforced with 40% glass fibers, without addition of any halogen compounds, red phosphorus and asbestos, doesn't release any toxic gases during burning..