Thermal Properties Metric English Comments
Vicat Softening Point 170 °C

@Load 1.02 kg
338 °F

@Load 2.25 lb
50°C/h; ISO 306
Styrolution Terblend® N NG-02 UV ABS / PA, 8% Glass filled
Terblend N NG-02 UV is an 8% glass fiber reinforced (UV stabilized) ABS/PA blend with enhanced dimensional stability and rigidity.High dimensional stabilityEnhanced rigidityEnhanced softening temper..