Polymer Property : Vicat Softening Point = 132 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Vicat Softening Point 132 °C

@Load 5.001 kg
270 °F

@Load 11.03 lb
50°C/h; ISO 306
Polykemi AB POLYfill PPH BF4075 VT1 Polypropylene Homopolymer, Reinforced, Heat Resistant
Information provided by Polykemi AB
Vicat Softening Point 132 °C

@Load 1.00 kg
270 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYlux 3809S PC/PBT-Blend
Information provided by Polykemi AB
Vicat Softening Point 132 °C

@Load 1.00 kg
270 °F

@Load 2.21 lb
50°C/h; ISO 306
Polykemi AB POLYlux 3809SLB PC/PBT-Blend, Paintable
Information provided by Polykemi AB
Vicat Softening Point 132 °C

@Load 1.02 kg
270 °F

@Load 2.25 lb
ISO 306
Borealis Daplen™ EE188HP Polypropylene TPO Compound
Daplen™ EE188HP is a 15% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness and g..
Vicat Softening Point 132 °C

@Load 5.00 kg
270 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND 0840 GF Polycarbonate ABS Blend, 20% Glass Filled
Polycarbonate and Acrylonitrile Butadiene Styrene blend with 20% glass fiber reinforcementHigh dimensional stability, high stiffnessInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 132 °C

@Load 5.00 kg
270 °F

@Load 11.0 lb
50°C/hr; ASTM D 1525
Cossa Polimeri ESTABLEND 8500 Polycarbonate ABS Blend
Polycarbonate and Acrylonitrile Butadiene Styrene blendHigh thermal resistance, high impact resistanceInformation provided by Cossa Polimeri S.r.l.
Vicat Softening Point 132 °C

@Load 5.10 kg
270 °F

@Load 11.2 lb
50°C/h; ISO 306
Covestro Bayblend® T88 GF-30 Rubber Modified PC Blend, 31% Glass Filled
Main characteristics:• High toughness even at low temperatures• High dimensional accuracy and stability• Good paintability• Good flowabilityGrade characteristics:• Rubber modified PC blend..