Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 45.0 °C @Load 5.10 kg |
113 °F @Load 11.2 lb |
ISO 306 |
Borealis EE002AE Polypropylene Elastomer Modified EE002AE is a reactor elastomer modified polypropylene compound intended for injection molding. The product is available in natural color. This material has excellent balanced mechanical properties.. |