Thermal Properties | Metric | English | Comments |
---|---|---|---|
Vicat Softening Point | 39.0 °C @Load 5.10 kg |
102 °F @Load 11.2 lb |
ISO 306 |
Borealis Daplen™ EE340AE Polypropylene TPO Compound Daplen™ EE340AE is a 30% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has excellent balanced mechanical properties, gives a good surface q.. |
|||
Vicat Softening Point | 39.0 °C @Load 5.10 kg |
102 °F @Load 11.2 lb |
ISO 306 |
Borealis Daplen™ EF005AE Polypropylene TPO Compound Daplen™ EF005AE is a 10% mineral filled elastomer modified polypropylene compound intended for injection molding. This material has an excellent balance between impact strength and stiffness, give.. |