Polymer Property : Maximum Service Temperature, Air = 849 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 849 °C
1560 °F
Aremco Pyro-Paint™ 634-BN (SC) High Temperature Refractory Coating
This highly-filled boron nitride solution is extremely lubricious and inert. It is non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN(SC) ..
Maximum Service Temperature, Air 849 °C
1560 °F
Aremco Pyro-Paint™ 634-BN High Temperature Refractory Coating
This highly-filled boron nitrite solution is extremely lubricious and inert. They are non-wetted by molten salts, glasses, plastics, and most metals including aluminum and magnesium. Select 634-BN f..