Thermal Properties Metric English Comments
Maximum Service Temperature, Air 84.4 °C
184 °F
Heat Distortion, Annealed; ASTM D648
Total PSI 830 Polystyrene
Polystyrene 830 is a high melt flow, high impact polystyrene specially designed for hard to fill injection molding applications. The high flow 830 material aids production of stress free parts.The m..