Polymer Property : Maximum Service Temperature, Air = 800.1 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 426.7 °C
800.1 °F
Pyrotek Pyroboard™ S400 Roller
Pyroboard™ S400 is a low temperature material that is normally used in cooling zones where water quenching is present.Information provided by Pyrotek.