Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 780 °C | 1440 °F | Not recommended for use in continuous casting applications. |
Pyrotek Pyrocast AR PLUS Castable Refractory Pyrocast AR Plus is a fused silica refractory castable inert to molten aluminum and its alloys. Parts cast from Pyrocast AR Plus are heat-treated to ensure that free and combined water are removed... |
|||
Maximum Service Temperature, Air | 780 °C | 1440 °F | |
Pyrotek RFM™ Autopour Ladle Light density refractory composite material ApplicationsHigh pressure die casting Gravity die casting Sand casting AdvantagesLight weight No pre-heating required Low thermal heat sink Excellent mechanical properties Excellent resistance to er.. |