Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 302 °C | 576 °F | Cured |
Parker Chomerics Tecknit TeckBond™-A Silver-Plated Aluminum-Filled Adhesive Description: TECKBOND-A conductive system is a silicone based, two-component RTV, filled with silver-plated aluminum particles. After cure, the resultant bond or seal is flexible, resilient, and con.. |