Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 566 °C | 1050 °F | Upper limit of working range |
Heatbath/Park Scale Kleen 5 Descaling Salt A highly alkaline and oxidizing salt bath mixture used for the non-electrolytic descaling of most ferrous alloys and conditioning of surface oxides for subsequent removal in dilute acid. Nickel, ch.. |