Thermal Properties Metric English Comments
Maximum Service Temperature, Air 285 °C
545 °F
Degradation Temp
Sanyo PELESTAT® NC6321 Antistatic Additive
PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a var..
Maximum Service Temperature, Air 285 °C
545 °F
Degradation Temp
Sanyo PELESTAT® NC7530 Antistatic Additive
PELESTAT® alloy type anti-static additives are true IDP (Inherent Dissipative Polymers) that give permanent static dissipation performance to thermoplastics. Pelestat® comes tailored to a var..