Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 238 °C | 460 °F | Continuous |
Pyrotek TS-107 Thermoset Electrical Insulation Product (Nema Grade: G-7) Glass reinforcement, Silicone resin, White color. High temperature resistance. Good electrical properties in humidity.ApplicationsSuperstructure support pads Bus bar insulators Pot cradle insulato.. |
|||
Maximum Service Temperature, Air | 238 °C | 460 °F | Heat distortion temperature, load unknown; ASTM D648 |
Mitsui AURUM® 450 Thermoplastic Polyimide Resin, Non-filled
(discontinued **) AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i.. |