Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 45.0 °C | 113 °F | Deflection Temp at unknown load |
Abatron AboCast 8503-7/AboCure 8503-7 Colorless Epoxy AboCast 8503-7/AboCure 8503-7 is a general purpose, slow hardening, colorless epoxy casting compound with low viscosity. It is similar to the 8503-4 system, but more flexible. Suggested Uses: Trans.. |