Songhan Plastic Technology Co.,Ltd.
 POLYMER SEARCH

Polymer Property : Maximum Service Temperature, Air = 440 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 227 °C
440 °F
UL-746 B
Saint-Gobain Norton® High Performance Extruded PEI Film
Description: PEI = polyetherimide. Used Primarily for Electrical/Electronics ApplicationsInformation provided by Saint Gobain Performance Products.
Copyright © lookpolymers.com All Rights Reserved