Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 190 - 216 °C | 374 - 421 °F | Average value: 202 °C Grade Count:15 |
Overview of materials for Phenolic, Novolac, Mineral/Flock Filled This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Flock Filled". Each property range of values reported is minimum and maximum .. |