Thermal Properties Metric English Comments
Maximum Service Temperature, Air 375 °C
707 °F
Intermittent
Atom Adhesives AA-BOND G298 Epoxy Adhesive
AA-BOND G298 is a two component, gold-filled, electrically and thermally conductive epoxy designed for hybrid microelectronic and semiconductor packaging.Appearance: Resin: Brown, Hardener: Dark Bro..
Maximum Service Temperature, Air 375 °C
707 °F
Intermittent
Atom Adhesives AA-SUPERTHERM 195 Epoxy Adhesive
AA-SUPERTHERM 195 is a two component, thermally conductive epoxy system recommended for staking transistors, diodes, resistors, integrated circuits and other heat sensitive components to printed cir..