Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 93.3 - 315 °C | 200 - 599 °F | Average value: 223 °C Grade Count:644 |
Overview of materials for Silicone Rubber This property data is a summary of similar materials in the MatWeb database for the category "Silicone Rubber". Each property range of values reported is minimum and maximum values of appropriate Ma.. |