Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 148 °C | 298 °F | Recommended |
Nye Lubricants 710R Grease Information provided by Nye Lubricants. |
|||
Maximum Service Temperature, Air | 148 °C | 298 °F | Short term |
3M 9453FL Adhesive Transfer Tape with 300LSE Adhesive Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS.. |
|||
Maximum Service Temperature, Air | 148 °C | 298 °F | Short term |
3M 9471FL Adhesive Transfer Tape with 300LSE Adhesive Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS.. |
|||
Maximum Service Temperature, Air | 148 °C | 298 °F | Short term |
3M 9472FL Adhesive Transfer Tape with 300LSE Adhesive Features:Clear Polyester (PET)Quick flowing acrylic adhesive speeds lamination processExcellent initial adhesion, especially to LSE (low surface energy) plasticsBonds graphics to powder coatings, LS.. |