Polymer Property : Maximum Service Temperature, Air = 2750 °F Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 1510 °C
2750 °F
Deformation under load - t<sub>a</sub>
Gouda Vuurvast AK 80 Dense Refractory Brick
Description: A bauxite based quality with a high abrasion resistance. Widely used in rotary cement kilns.Remarks: This data represents average values, obtained from samples that were cut from standa..
Maximum Service Temperature, Air 1510 °C
2750 °F
Gouda Vuurvast GI 28 Insulating Refractory Brick
This data represents average values, obtained from samples that were cut from standard bricks.Information provided by Gouda Vuurvast.
Maximum Service Temperature, Air 1510 °C
2750 °F
Thermal Ceramics MRI FS-85P Pre-Fired Refractory Shapes
MRI pressed fired shapes are used in a variety of alloy melt-pour systems. The pressed manufacture process meets the tight tolerance specifications required by end users. Precise size dies and detai..
Maximum Service Temperature, Air 1510 °C
2750 °F
Thermal Ceramics MRI FS-85V Pre-Fired Refractory Shapes
MRI pressed fired shapes are used in a variety of alloy melt-pour systems. The pressed manufacture process meets the tight tolerance specifications required by end users. Precise size dies and detai..