Thermal Properties Metric English Comments
Maximum Service Temperature, Air 245 °C
473 °F
Heat distortion temperature, load unknown; ASTM D648
Mitsui AURUM® JGN3030 Thermoplastic Polyimide Resin, Amorphous  (discontinued **)
AURUM® is an easy melt, processable and recyclable thermoplastic polyimide resin that provides continuous service temperatures to 465° F in its amorphous state and up to 550° F when annealed to i..
Maximum Service Temperature, Air 245 °C
473 °F
Continuous
GrafTech GRAFOIL® UCAR®-323 Reinforced PTFE Gasketing
GRAFOIL® Grade UCAR®-323 is a laminated gasket material consisting of multiple plies of woven fiberglass coated with PTFE. It will not support combustion or bacteria. Its applications include:..