Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 222 °C | 432 °F | Heat Resistance; ASTM D570D |
Plenco 08218 Polyester BMC, Compression Molded PLENCO 08218 is a renumber of PlasGlas 20118. PLENCO 08218 is an 18% glass-filled polyester bulk molding compound characterized as an electrical grade, but has many outstanding properties that make .. |