Polymer Property : Maximum Service Temperature, Air = 21.1 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 21.1 - 371 °C
70.0 - 700 °F
Average value: 120 °C Grade Count:340
Overview of materials for Cyanoacrylate Adhesive
This property data is a summary of similar materials in the MatWeb database for the category "Cyanoacrylate Adhesive". Each property range of values reported is minimum and maximum values of appropr..
Maximum Service Temperature, Air 21.1 °C
70.0 °F
Dielectric Polymers NT-988-2 Overlap Splice Tape  (discontinued **)
Acrylic copolymer adhesive with silicone treated release paper backing.Features: Chemical resistantGood conformabilityPlasticizer migration resistantExcellent adhesion to low surface energy substrat..
Maximum Service Temperature, Air 21.1 °C
70.0 °F
Dielectric Polymers NT4500 Protective Film  (discontinued **)
Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA..
Maximum Service Temperature, Air 21.1 °C
70.0 °F
Dielectric Polymers NT-4502 Protective Film  (discontinued **)
Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA..
Maximum Service Temperature, Air 21.1 °C
70.0 °F
Dielectric Polymers NT-5000 Protective Film  (discontinued **)
Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA..
Maximum Service Temperature, Air 21.1 °C
70.0 °F
BCC Products KRYTOX V-116 Mold Release Agent
KRYTOX SPRAY V-116 is a dry, waxy mold release. It is an anti-sick and paintable. It is ideal for use in a broad variety of applications, such as plastic injection molding. Rigid, semi-rigid and fle..
Maximum Service Temperature, Air 21.1 °C
70.0 °F
Dielectric Polymers NT-988 High Tack Laminating Adhesive  (discontinued **)
Acrylic copolymer adhesive with silicone treated release paper liner.Features: Excellent adhesion to low surface energy substratesCompatible with most printing inksApplications: Mounting a wide vari..
Maximum Service Temperature, Air 21.1 °C
70.0 °F
Dielectric Polymers NT-5002 Protective Film  (discontinued **)
Acrylic adhesive with polyester film backing.Features: Clean removal even after exposure to high and low temperaturesSolvent resistantMoisture resistantFor use on matte metals and textured plasticsA..