Polymer Property : Maximum Service Temperature, Air = 203 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 196 - 203 °C
385 - 397 °F
Average value: 201 °C Grade Count:5
Overview of materials for Phenolic, Novolac, Mineral/Cellulose Filled
This property data is a summary of similar materials in the MatWeb database for the category "Phenolic, Novolac, Mineral/Cellulose Filled". Each property range of values reported is minimum and maxi..