Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 86.7 °C | 188 °F | Heat Distortion, Annealed; ASTM D648 |
Total PSC 500 Polystyrene Polystyrene 500 is a high melt, easy flow crystal polystyrene for fast cycle injection molding. The high flow characteristics of this material make it easy to fill thin parts. 500 is utilized in pro.. |