Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 165 - 175 °C | 329 - 347 °F | Softening Range |
Huntsman HT 9719-1 Aromatic Amine Approx. H+ equivalent weight 63. Mix Ratio with GY 6010 is 36.Comments/Applications: 3,3' -diaminodiphenyl sulfone, micropulverized, solid amine. Composites, adhesives.Data provided by Ciba Speci.. |