Polymer Property : Maximum Service Temperature, Air = 161 °C Product List

Thermal Properties

Tips: 30 items are displayed at most. For the rest of the results, please contact customer service.
Thermal Properties Metric English Comments
Maximum Service Temperature, Air 161 °C
322 °F
Cured
Parker Chomerics Tecknit® 73-00008 Electrically Conductive Acrylic and Polyurethane Paint
Description: TECKNIT manufactures a highly conductive acrylic and polyurethane paints filled with silver. These coatings provide a cost effective method for shielding and grounding plastic enclosure..
Maximum Service Temperature, Air 161 °C
322 °F
Heat deflection temperature, load unknown; ASTM D648
Toyobo PELPRENE™ PE450B Polyester TPE
Features: Polyester TPEInformation provided by Toyobo.