Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 150 - 154 °C | 302 - 310 °F | Average value: 150 °C Grade Count:11 |
Overview of materials for Modified ETFE, Unreinforced This property data is a summary of similar materials in the MatWeb database for the category "Modified ETFE, Unreinforced". Each property range of values reported is minimum and maximum values of ap.. |