Thermal Properties | Metric | English | Comments |
---|---|---|---|
Maximum Service Temperature, Air | 1538 °C | 2800 °F | Recommended Operating Temperature |
Unifrax Fiberwall® Bonded 30 Bonded Module System Fiberfrax Bonded modules and Hefty-Loc alloy steel hardware are the components of the Hefty-Loc module lining system. The Hefty-Loc system provides an insulation lining for a variety of heat proces.. |
|||
Maximum Service Temperature, Air | 1538 °C | 2800 °F | Recommended Operating Temperature |
Unifrax Foamfrax® Grade III Fiber Insulation Foamfrax® Insulation is a monolithic insulation system developed by Unifrax. Foamfrax Insulation is a three-component system of specially conditioned bulk ceramic or soluble fibers, an inorganic b.. |
|||
Maximum Service Temperature, Air | 1538 °C | 2800 °F | Recommended Operating Temperature |
Unifrax Foamfrax® HD Grade III Fiber HD Insulation Foamfrax® HD Insulation is a monolithic thermal management product developed by Unifrax Corporation. This product is a four-component system of specially conditioned bulk ceramic fibers, an inorga.. |
|||
Maximum Service Temperature, Air | 1538 °C | 2800 °F | Normal oxidizing atmosphere |
BNZ Materials BNZ-28 Insulating Firebrick BNZ produces many types of Insulating Fire Brick (IFB) for use in applications from 2,000°F (1,093°C) to 3,200°F (1,760°C). Each type is formulated to meet specific thermal and physical requirem.. |